Title: Reinforced Concrete Beam-Column Joints Under Seismic Actions

Author(s): T. Paulay, R. Park, and M. J. N. Preistley

Publication: Journal Proceedings

Volume: 75

Issue: 11

Appears on pages(s): 585-593

Keywords: anchorage (structural);axial loads;beam-column frame;beams (supports); columns (supports);connections;cracking (fracturing);cylic loads; deformation; earthquake resistant structures;earthquakes;hinges (structural);joints (junctions); prestressed concrete.

DOI: 10.14359/10971

Date: 11/1/1978

Abstract:
The behavior of interior beam-column joints unders seismic actions is examined in detail. The exisitance of two shear resisting mechanisms, one involving joint shear einforcement and the other a linear concrete strut, is postulated and the effects of reversed cyclic loading on these mechanisms, in both elastic and inelastic range of response, are discussed. Simple analytical models of behavior are presented. The determental effects of yield penetration into a joint upon longitudinal bar anchorage are discussed, and methods to overcome these effects are proposed.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer