Title: Comparative Study of Predictions of Flexural Strength of Steel Fiber Concrete

Author(s): H. V. Dwarakanath and T. S. Nagaraj

Publication: Structural Journal

Volume: 88

Issue: 6

Appears on pages(s): 714-720

Keywords: compressive strength; concrete slabs; fiber reinforced concrete; flexural strength; metal fibers; prisms; tensile strength; Structural Research

DOI: 10.14359/1262

Date: 11/1/1992

Abstract:
Several methods are available for predicting flexural strength of steel fiber concrete composites. In these methods, direct tensile strength, split cylinder strength, and cube strength are the basic engineering parameters that must be determined to predict the flexural strength of such composites. Various simplified forms of stress distribution are used in each method to formulate the prediction equations for flexural strength. In this paper, existing methods are reviewed and compared, and a modified empirical approach is developed to predict the flexural strength of fiber concrete composites. The direct tensile strength of the composite is used as the basic parameter in this approach. Stress distribution is established from the findings of flexural tests conducted as part of this investigation on fiber concrete prisms. A comparative study of the test values of an earlier investigation on fiber concrete slabs and the computed values from existing methods, including the one proposed, is presented.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.