Title: Bond Stress Versus Slip Relationship and Cracking Response of Tension Members

Author(s): S. Somayaji and S. P. Shah

Publication: Journal Proceedings

Volume: 78

Issue: 3

Appears on pages(s): 217-225

Keywords: bond stress; cracking (fracturing); crack width and spacing; mathematical models; reinforced concrete; slippage; stiffness; structural analysis; tension; tension tests.

DOI: 10.14359/6920

Date: 5/1/1981

Abstract:
An analytical model is proposed to predict the cracking response and the tension-stiffening effect in a reinforced concrete member subjected to uniaxial tension. Instead of assuming a bond stress versus slip relationship, a function was assumed to represent the bond stress distribution. To check the validity of the analytical predictions, an experimental investigation was conducted on reinforced mortar specimens subjected to uniaxial tension. Measurements of elongations and crack widths were made during testing. The results of the theoretical predictions were also compared satisfactorily with some available experimental data on reinforced concrete prisms. The proposed method can be used in the application of finite element method to analyze the behavior of reinforced concrete members.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer