Title:
Analytical Model for Predicting Shear Strengths of Exterior Reinforced Concrete Beam-Column Joints for Seismic Resistance
Author(s):
Shyh-Jiann Hwang and Hung-Jen Lee
Publication:
Structural Journal
Volume:
96
Issue:
5
Appears on pages(s):
846-858
Keywords:
beams; columns; joints (junctions); reinforced concretes; shear; strength
DOI:
10.14359/739
Date:
9/1/1999
Abstract:
A proposal for determining the shear strengths of exterior beam-column joints for seismic resistance is made in this paper. The proposed method, termed as the softened strut-and-tie model, is based on the strut-and-tie concept and derived to satisfy equilibrium, compatibility, and the constitutive laws of cracked reinforced concrete. The accuracy of the proposed procedure was checked by comparing calculated shear strengths with experimental data reported in previous literature, and a satisfactory correlation was found. The proposed physical model can provide valuable insights into the strength behavior of the exterior beam-column joints under seismic loading.