Title:
Inelastic Behavior and Fracture of Concrete
Author(s):
Surendra P. Shah and George Winter
Publication:
Journal Proceedings
Volume:
63
Issue:
9
Appears on pages(s):
925-930
Keywords:
cracking, fracture mechanics, microcracking, research, shorttime loading, stress-strain curve.
DOI:
10.14359/7659
Date:
9/1/1966
Abstract:
Elements of a unified theory of the mechanical behavior of concrete, from no-load to fracture under short-time load-ing, are developed, based observed microcrack behavior and on a statistical distribution of mortar strength.