Email Address is required Invalid Email Address
In todayโs market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have itโฆthey are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Tools > Frequently Asked Questions
Q. Is the cutting of cores or other shaped specimens directly from a completed structure ever used for determining the strength of the concrete? A. Yes. This is a widely accepted procedure both for routine control and for special investigations where the condition of a structure is in question. References: SP-1(02); ACI PRC-214.4-21 Topics in Concrete: Quality Assurance; Testing of Concrete
Q. Is the cutting of cores or other shaped specimens directly from a completed structure ever used for determining the strength of the concrete?
A. Yes. This is a widely accepted procedure both for routine control and for special investigations where the condition of a structure is in question.
References: SP-1(02); ACI PRC-214.4-21
Topics in Concrete: Quality Assurance; Testing of Concrete