ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. How is time of setting of concrete measured? A. There are several methods for measuring setting time, among them are the following: - Standard Test Methods for Time of Setting of Hydraulic Cement by Vicat Needle (ASTM C191) - Standard Test Method for Time of Setting of Concrete Mixtures by Penetration Resistance (ASTM C403) - Standard Test Method for Time of Setting of Hydraulic-Cement Paste by Gillmore Needles (ASTM C266) - Standard Test Method for Time of Setting of Grouts for Preplaced-Aggregate Concrete in the Laboratory (ASTM C953) References: SP-1(02); ACI Physical Testing of Cement Training Video; ASTM C403; ASTM C191; ASTM C266; ASTM C953 Topics in Concrete: Cementitious Material; Concrete Fundamentals; Materials
Q. How is time of setting of concrete measured?
A. There are several methods for measuring setting time, among them are the following:
- Standard Test Methods for Time of Setting of Hydraulic Cement by Vicat Needle (ASTM C191)
- Standard Test Method for Time of Setting of Concrete Mixtures by Penetration Resistance (ASTM C403)
- Standard Test Method for Time of Setting of Hydraulic-Cement Paste by Gillmore Needles (ASTM C266)
- Standard Test Method for Time of Setting of Grouts for Preplaced-Aggregate Concrete in the Laboratory (ASTM C953)
References: SP-1(02); ACI Physical Testing of Cement Training Video; ASTM C403; ASTM C191; ASTM C266; ASTM C953
Topics in Concrete: Cementitious Material; Concrete Fundamentals; Materials