ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. How can it be determined that an admixture will serve its intended purpose? A. The best way is to test it with the concrete materials to be used in the work and carefully measure the properties of interest in similar mixtures with and without recommended dosages of the proposed admixture, but at similar slump and air content. Concrete and ambient temperatures should also be representative of job conditions. ASTM C233 and C260 describe such tests and provide specifications for air-entraining admixtures. ASTM C494 and C1017 do the same for chemical admixtures for water reduction, retardation, and acceleration. When time or other conditions do not permit proper testing, the service record of the admixture with similar materials, especially the cementitious materials, should be thoroughly investigated. If the work has started, job tests have some value, but they rarely have the control and precision of laboratory work. Moreover, laboratory tests made well in advance of construction allow time for strength tests at later ages as well as for tests of other properties of the hardened concrete, such as resistance to freezing and thawing and chloride penetration. References: SP-1(02); CCS-0(16); ACI CT-23; E4-22; ACI 212.3R-16; SP-288; ASTM C260; ASTM C494; ASTM C1017 Topics in Concrete: Admixture; Quality Assurance; Testing of Concrete; Specifications
Q. How can it be determined that an admixture will serve its intended purpose?
A. The best way is to test it with the concrete materials to be used in the work and carefully measure the properties of interest in similar mixtures with and without recommended dosages of the proposed admixture, but at similar slump and air content. Concrete and ambient temperatures should also be representative of job conditions. ASTM C233 and C260 describe such tests and provide specifications for air-entraining admixtures. ASTM C494 and C1017 do the same for chemical admixtures for water reduction, retardation, and acceleration.
When time or other conditions do not permit proper testing, the service record of the admixture with similar materials, especially the cementitious materials, should be thoroughly investigated. If the work has started, job tests have some value, but they rarely have the control and precision of laboratory work. Moreover, laboratory tests made well in advance of construction allow time for strength tests at later ages as well as for tests of other properties of the hardened concrete, such as resistance to freezing and thawing and chloride penetration.
References: SP-1(02); CCS-0(16); ACI CT-23; E4-22; ACI 212.3R-16; SP-288; ASTM C260; ASTM C494; ASTM C1017