ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. What allowance should be made for strengths where air-entrained concrete is to be used? A. For a given required average strength, ACI 211.1 recommends a substantially lower w/cm for air-entrained concrete than for non-air-entrained concrete. These values should be used until experience with the given materials indicates that a change can be safely made. Experience has shown that when the cementitious material content and consistency are maintained constant, the apparent penalty in strength is partially or entirely offset by the reduction in mixing water requirements, which results from the better workability obtained by air entrainment (ACI 212.3R). For concretes with low cementitious material content, air entrainment may actually result in higher strength for a given workability and cementitious material content. References: SP-1(02); ACI PRC-211.1-22; ACI 212.3R-16 Topics in Concrete: Admixture; Mixture Proportioning
Q. What allowance should be made for strengths where air-entrained concrete is to be used?
A. For a given required average strength, ACI 211.1 recommends a substantially lower w/cm for air-entrained concrete than for non-air-entrained concrete. These values should be used until experience with the given materials indicates that a change can be safely made. Experience has shown that when the cementitious material content and consistency are maintained constant, the apparent penalty in strength is partially or entirely offset by the reduction in mixing water requirements, which results from the better workability obtained by air entrainment (ACI 212.3R). For concretes with low cementitious material content, air entrainment may actually result in higher strength for a given workability and cementitious material content.
References: SP-1(02); ACI PRC-211.1-22; ACI 212.3R-16
Topics in Concrete: Admixture; Mixture Proportioning