ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. How is the temperature of concrete measured? A. ASTM C1064 is the standard test method to measure temperature of freshly mixed concrete. The temperature is read from a temperature measuring device inserted into the concrete. Temperature affects the rate of hydration. References: SP-1(02); ACI 209R-92; ASTM C1064 Topics in Concrete: Concrete Fundamentals; Hot Weather; Mass Concrete; Testing of Concrete
Q. How is the temperature of concrete measured?
A. ASTM C1064 is the standard test method to measure temperature of freshly mixed concrete. The temperature is read from a temperature measuring device inserted into the concrete. Temperature affects the rate of hydration.
References: SP-1(02); ACI 209R-92; ASTM C1064
Topics in Concrete: Concrete Fundamentals; Hot Weather; Mass Concrete; Testing of Concrete