ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. How is the resistance to freezing and thawing determined? A. Resistance to freezing and thawing is determined by ASTM C666, ASTM C671, and ASTM C682. Scaling resistance is determined by ASTM C672. References: SP-1(02); ASTM C666; ASTM C671; ASTM C672; ASTM C682; Topics in Concrete: Testing of Concrete
Q. How is the resistance to freezing and thawing determined?
A. Resistance to freezing and thawing is determined by ASTM C666, ASTM C671, and ASTM C682. Scaling resistance is determined by ASTM C672.
References: SP-1(02); ASTM C666; ASTM C671; ASTM C672; ASTM C682;
Topics in Concrete: Testing of Concrete