ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. Would adding more cement serve the purpose of admixtures? A. In general, no. Adding more cement is effective only in cases where more cement may improve workability and reduce the w/cm, provided these improvements can be obtained to the desired degree for the same cost. Also, more cement can be effective in cold weather to raise heat of hydration. More cement will not retard the time of setting in warm weather, nor will it entrain air. Neither will it reduce the heat of hydration and temperature rise within mass concrete, as some admixtures will when they make it possible to reduce the cement content. Also, more cement with more water would result in more drying shrinkage. References: SP-1(02); CCS-0(16); E4-22; ACI 212.3R-16; SP-288; ACI 209.1R-05; ACI 207.1R-05 Topics in Concrete: Admixture for Concrete; Durability of Concrete; Materials in Concrete; Mass Concrete; Shrinkage-Compensating Concrete
Q. Would adding more cement serve the purpose of admixtures?
A. In general, no. Adding more cement is effective only in cases where more cement may improve workability and reduce the w/cm, provided these improvements can be obtained to the desired degree for the same cost. Also, more cement can be effective in cold weather to raise heat of hydration. More cement will not retard the time of setting in warm weather, nor will it entrain air. Neither will it reduce the heat of hydration and temperature rise within mass concrete, as some admixtures will when they make it possible to reduce the cement content. Also, more cement with more water would result in more drying shrinkage.
References: SP-1(02); CCS-0(16); E4-22; ACI 212.3R-16; SP-288; ACI 209.1R-05; ACI 207.1R-05
Topics in Concrete: Admixture for Concrete; Durability of Concrete; Materials in Concrete; Mass Concrete; Shrinkage-Compensating Concrete