ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Frequently Asked Questions
In This Section
Frequently Asked Questions
Submit a Question
Search other resources on the ACI website for answers to technical questions
Q. Do some water-reducing admixtures induce bleeding? A. Yes, some do, and this may be beneficial in concrete for flatwork in a hot, arid climate by minimizing plastic shrinkage. Bleeding is the rise of the mixing water in newly placed concrete. Plastic shrinkage occurs when the rate of evaporation exceeds the rate of bleeding. Bleeding may reduce strength and increase permeability if the bleed water is worked into the surface. Bleed water lost by evaporation reduces the w/cm and raises the strength of concrete. References: SP-1(02); CCS-0(16); E4-22; ACI 212.3R-16; SP-288; ASTM C494; ASTM C1017 Topics in Concrete: Admixture; Concrete Fundamentals; Materials
Q. Do some water-reducing admixtures induce bleeding?
A. Yes, some do, and this may be beneficial in concrete for flatwork in a hot, arid climate by minimizing plastic shrinkage. Bleeding is the rise of the mixing water in newly placed concrete. Plastic shrinkage occurs when the rate of evaporation exceeds the rate of bleeding. Bleeding may reduce strength and increase permeability if the bleed water is worked into the surface. Bleed water lost by evaporation reduces the w/cm and raises the strength of concrete.
References: SP-1(02); CCS-0(16); E4-22; ACI 212.3R-16; SP-288; ASTM C494; ASTM C1017