Abstract:
Development of probability-based second moment codes of several types is currently taking place. The paper describes the general philosophy of developing such codes. Various probability based improvements are suggested for the current ACI code. Some of the problems associated with the introduction of probabilistic concepts in current codes are described.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer