Title: 
            Concrete Bridge Articulation
        
        
            Author(s): 
            H. B. Day
        
        
            
                Publication: 
                Symposium Paper
            
            
                Volume: 
                70
            
            
                Issue: 
                
            
            
                Appears on pages(s): 
                55-76
            
            
                Keywords: 
                bridge bearings; bridge piers; bridges (structures); elastic analysis; loads (forces); plastics, polymers and resins; stiffness; structural analysis; structural design; substructures; superstructures.
            
            
                DOI: 
                10.14359/17402
            
        
        
            Date: 
            1/1/1981
        
        
            Abstract:
            This paper demonstrates to bridge designers the advantages of matching bearing stiffness to pier stiffness to achieve economic load sharing of longitudinal loads on concrete bridges. The paper discusses the types of bearings and their limitations for articulation, bridge movements and horizontal loads, and sets out the design process for a bridge supported and restrained by elastomeric bearings only -- an elastically restrained structure. An example of the calculations at a typical pier is given.  The following articulation systems for a continuous bridge example are analysed, the results tabulated and compared:         pinned and sliding, tmnolithic and elastomeric,        pinned and elastomeric, all elastomeric bearings  The following articulation systems for a simply supported bridge example are analysed, the results tabulated and compared: pinned and sliding, pinned and elastomeric, all elastomeric bearings. The paper concludes that matching bearing stiffness to pier stiffness produces cost savings; that elastomeric bearings are superior for this purpose, that elastically restrained bridges give the best load sharing amongst piers and that load sharing can be improved with sliding bearings by varying the coefficient of friction.