Title:
Crushing Behavior and Crushing Strengths of Low-Density Foam Concrete
Author(s):
Yu Song and David A. Lange
Publication:
Materials Journal
Volume:
117
Issue:
2
Appears on pages(s):
43-52
Keywords:
cellular concrete; cellular material; crushable foam; crushing strength; foam concrete; foam material; foam modulus; mechanical property
DOI:
10.14359/51722394
Date:
3/1/2020
Abstract:
Foam concrete is a highly cellularized cementitious material that undergoes extensive plastic deformation when loaded to failure. Under compression, the microstructure of low-density foam concrete gets progressively crushed at a steady stress stage, accompanied by substantial energy dissipation. Understanding foam concrete crushing behavior is of special importance for its engineering applications. However, the current studies are insufficient to define key attributes that are important for material characterization and design. This study focuses on low-density foam concrete ranging from 0.4 to 0.8 g/cm3 (25 to 50 lb/ft3), with the crushing behavior investigated using a penetration test and dynamic Young’s modulus determined using a resonant frequency test. Four distinct crushing phases—linear elastic, transitional, plateau, and final densification—are observed for the samples. Furthermore, the yield strength and plateau strength are identified to characterize the foam crushing behavior. Using the experimental inputs, the modulus-strength constitutive relationship is established for predicting the crushing behavior with fundamental material properties. The findings significantly facilitate subsequent foam concrete studies, as well as the engineering design of this material.
Related References:
1. ACI Committee 523, “Guide for Cellular Concretes above 50 lb/ft3 (800 kg/m3) (ACI 523.3R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 17 pp.
2. ACI Committee 229, “Report on Controlled Low-Strength Materials (ACI 229R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 22 pp.
3. Jones, M. R., and McCarthy, A., “Behaviour and Assessment of Foamed Concrete for Construction Applications,” Use of Foamed Concrete in Construction, 2005, pp. 62-88.
4. Jones, M. R., and McCarthy, A., “Preliminary Views on the Potential of Foamed Concrete as a Structural Material,” Magazine of Concrete Research, V. 57, No. 1, 2005, pp. 21-31. doi: 10.1680/macr.2005.57.1.21
5. Wei, S.; Yunsheng, Z.; and Jones, M. R., “Using the Ultrasonic Wave Transmission Method to Study the Setting Behavior of Foamed Concrete,” Construction and Building Materials, V. 51, 2014, pp. 62-74. doi: 10.1016/j.conbuildmat.2013.10.066
6. Jones, M. R.; Ozlutas, K.; and Zheng, L., “Stability and Instability of Foamed Concrete,” Magazine of Concrete Research, V. 68, No. 11, 2016, pp. 542-549. doi: 10.1680/macr.15.00097
7. Zhang, Z. Q.; Yang, J. L.; and Li, Q. M., “An Analytical Model of Foamed Concrete Aircraft Arresting System,” International Journal of Impact Engineering, V. 61, 2013, pp. 1-12. doi: 10.1016/j.ijimpeng.2013.05.006
8. Santagata, E.; Bassani, M.; and Sacchi, E., “Performance of New Materials for Aircraft Arrestor Beds,” Transportation Research Record: Journal of the Transportation Research Board, V. 2177, No. 1, 2010, pp. 124-131. doi: 10.3141/2177-15
9. Wang, J.; Guo, W.; Zhao, R.; Shi, Y.; and Zeng, L., “Energy-Absorbing Properties and Crushing Flow Stress Equation of Lightweight Foamed Concrete,” Journal of Civil, Architectural & Environmental Engineering, V. 35, No. 6, 2013, pp. 97-102.
10. Jiang, C.; Yao, H.; Xiao, X.; Kong, X.; and Shi, Y., “Phenomena of Foamed Concrete under Rolling of Aircraft Wheels,” Journal of Physics: Conference Series, V. 495, 2014, p. 012035 doi: 10.1088/1742-6596/495/1/012035
11. Bing, C.; Zhen, W.; and Ning, L., “Experimental Research on Properties of High-Strength Foamed Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 1, 2012, pp. 113-118. doi: 10.1061/(ASCE)MT.1943-5533.0000353
12. Amran, Y. H. M.; Farzadnia, N.; and Ali, A. A. A., “Properties and Applications of Foamed Concrete; A Review,” Construction and Building Materials, V. 101, 2015, pp. 990-1005. doi: 10.1016/j.conbuildmat.2015.10.112
13. Nambiar, E. K. K., and Ramamurthy, K., “Shrinkage Behavior of Foam Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 21, No. 11, 2009, pp. 631-636. doi: 10.1061/(ASCE)0899-1561(2009)21:11(631)
14. Narayanan, N., and Ramamurthy, K., “Structure and Properties of Aerated Concrete: A Review,” Cement and Concrete Composites, V. 22, No. 5, 2000, pp. 321-329. doi: 10.1016/S0958-9465(00)00016-0
15. Ramamurthy, K.; Kunhanandan Nambiar, E. K.; and Indu Siva Ranjani, G., “A Classification of Studies on Properties of Foam Concrete,” Cement and Concrete Composites, V. 31, No. 6, 2009, pp. 388-396. doi: 10.1016/j.cemconcomp.2009.04.006
16. Valore, R. C. Jr., “Cellular Concretes Part 2 Physical Properties,” ACI Journal Proceedings, V. 50, No. 6, June 1954, pp. 817-836.
17. Byun, K.; Song, H.; Park, S.; and Song, Y., “Development of Structural Lightweight Foamed Concrete Using Polymer Foam Agent,” Icpic-98, 1998.
18. Jones, M. R., and McCarthy, A., “Heat of Hydration in Foamed Concrete: Effect of Mix Constituents and Plastic Density,” Cement and Concrete Research, V. 36, No. 6, 2006, pp. 1032-1041. doi: 10.1016/j.cemconres.2006.01.011
19. Fujiwara, H., Sawada, E.; and Ishikawa, Y., “Manufacture of High-Strength Aerated Concrete Containing Silica Fume,” Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete: Proceedings, 5th International Conference, SP-153, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1995, pp. 779-794.
20. De Rose, L., and Morris, J., “The Influence of Mix Design on the Properties of Microcellular Concrete,” Thomas Telford, London, UK, 1999, pp. 185-197.
21. Huang, Z.; Zhang, T.; and Wen, Z., “Proportioning and Characterization of Portland Cement-Based Ultra-Lightweight Foam Concretes,” Construction and Building Materials, V. 79, 2015, pp. 390-396. doi: 10.1016/j.conbuildmat.2015.01.051
22. Kearsley, E. P., and Wainwright, P. J., “The Effect of High Fly Ash Content on the Compressive Strength of Foamed Concrete,” Cement and Concrete Research, V. 31, No. 1, 2001, pp. 105-112. doi: 10.1016/S0008-8846(00)00430-0
23. Tarasov, A. S.; Kearsley, E. P.; Kolomatskiy, A. S.; and Mostert, H. F., “Heat Evolution Due to Cement Hydration in Foamed Concrete,” Magazine of Concrete Research, V. 62, No. 12, 2010, pp. 895-906. doi: 10.1680/macr.2010.62.12.895
24. Panesar, D. K., “Cellular Concrete Properties and the Effect of Synthetic and Protein Foaming Agents,” Construction and Building Materials, V. 44, 2013, pp. 575-584. doi: 10.1016/j.conbuildmat.2013.03.024
25. Kearsley, E. P., and Booysens, P., “Reinforced Foamed Concrete—Can It Be Durable?” Concrete/Beton, No. 91, 1998, pp. 5-9.
26. Nambiar, E. K. K., and Ramamurthy, K., “Influence of Filler Type on the Properties of Foam Concrete,” Cement and Concrete Composites, V. 28, No. 5, 2006, pp. 475-480. doi: 10.1016/j.cemconcomp.2005.12.001
27. Nambiar, E. K. K., and Ramamurthy, K., “Models Relating Mixture Composition to the Density and Strength of Foam Concrete Using Response Surface Methodology,” Cement and Concrete Composites, V. 28, No. 9, 2006, pp. 752-760. doi: 10.1016/j.cemconcomp.2006.06.001
28. Lim, S. K.; Tan, C. S.; Li, B.; Ling, T.-C.; Hossain, M. U.; and Poon, C. S., “Utilizing High Volumes Quarry Wastes in the Production of Lightweight Foamed Concrete,” Construction and Building Materials, V. 151, 2017, pp. 441-448. doi: 10.1016/j.conbuildmat.2017.06.091
29. Kearsley, E. P., and Wainwright, P. J., “Ash Content for Optimum Strength of Foamed Concrete,” Cement and Concrete Research, V. 32, No. 2, 2002, pp. 241-246. doi: 10.1016/S0008-8846(01)00666-4
30. Jones, M. R., and McCarthy, A., “Utilising Unprocessed Low-Lime Coal Fly Ash in Foamed Concrete,” Fuel, V. 84, No. 11, 2005, pp. 1398-1409. doi: 10.1016/j.fuel.2004.09.030
31. She, W.; Du, Y.; Zhao, G.; Feng, P.; Zhang, Y.; and Cao, X., “Influence of Coarse Fly Ash on the Performance of Foam Concrete and Its Application in High-Speed Railway Roadbeds,” Construction and Building Materials, V. 170, 2018, pp. 153-166. doi: 10.1016/j.conbuildmat.2018.02.207
32. McCormick, F., “Rational Proportioning of Preformed Foam Cellular Concrete,” ACI Journal Proceedings, V. 64, No. 2, Feb. 1967, pp. 104-110.
33. Song, Y., and Lange, D., “Measuring Young’s Modulus of Low-Density Foam Concrete Using Resonant Frequency,” Preprints, 2019.
34. Gibson, L. J., and Ashby, M. F., Cellular Solids, Cambridge University Press, Cambridge, UK, 1999.
35. Ashby, M. F., and Medalist, R. F. M., “The Mechanical Properties of Cellular Solids,” Metallurgical Transactions. A, Physical Metallurgy and Materials Science, V. 14, No. 9, 1983, pp. 1755-1769. doi: 10.1007/BF02645546
36. Birchall, J. D.; Howard, A. J.; and Kendall, K., “Flexural Strength and Porosity of Cements,” Nature, V. 289, 1981, pp. 388-390.
37. Yusuf, I. T.; Jimoh, Y. A.; and Salami, W. A., “An Appropriate Relationship between Flexural Strength and Compressive Strength of Palm Kernel Shell Concrete,” Alexandria Engineering Journal, V. 55, No. 2, 2016, pp. 1553-1562.
38. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.
39. ASTM C796-12, “Foaming Agents for Use in Producing Cellular Concrete Using Preformed Foam 1,��� ASTM International, West Conshohocken, PA, 2012, 12 pp.
40. ASTM C305-14, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2014, 3 pp.
41. Zhou, Q., and Mayer, R. R., “Characterization of Aluminum Honeycomb Material Failure in Large Deformation Compression, Shear, and Tearing,” Journal of Engineering Materials and Technology, V. 124, No. 4, 2002, pp. 412-420. doi: 10.1115/1.1491575
42. Ramamurty, U., and Kumaran, M. C., “Mechanical Property Extraction through Conical Indentation of a Closed-Cell Aluminum Foam,” Acta Materialia, V. 52, No. 1, 2004, pp. 181-189. doi: 10.1016/j.actamat.2003.09.004
43. Reddy, T. Y.; Wen, H. M.; Reid, S. R.; and Soden, P. D., “Dynamic Perforation of Composite Sandwich Panels by Projectiles with Hemispherical and Conical Tips,” Structures Under Extreme Loading Conditions, American Society of Mechanical Engineers, New York, 1997, pp. 151-164.
44. Wen, H. M.; Reddy, T. Y.; Reid, S. R.; and Soden, P. D., “Indentation, Penetration and Perforation of Composite Laminate and Sandwich Panels under Quasi-Static and Projectile Loading,” Key Engineering Materials, V. 141-143, 1998, pp. 501-552.
45. Barsotti, M. A.; Puryear, J. M. H.; and Stevens, D. J., Developing Improved Civil Aircraft Arresting Systems, National Academies Press, Washington, DC, 2009, 66 pp.
46. ASTM C215-14, “Standard Test Method for Fundamental Transverse, Longitudinal, and Torsional Resonant Frequencies of Concrete Specimens 1,” ASTM International, West Conshohocken, PA, 2014, 7 pp.
47. Hooton, R.; Kolluru, S.; Popovics, J.; and Shah, S. P., “Determining Elastic Properties of Concrete Using Vibrational Resonance Frequencies of Standard Test Cylinders,” Cement, Concrete and Aggregates, V. 22, No. 2, 2000, p. 81 doi: 10.1520/CCA10467J
48. Murthy, T. G.; Huang, C.; and Chandrasekar, S., “Characterization of Deformation Field in Plane-Strain Indentation of Metals,” Journal of Physics. D, Applied Physics, V. 41, No. 7, 2008, p. 074026 doi: 10.1088/0022-3727/41/7/074026
49. Murthy, T. G.; Saldana, C.; Hudspeth, M. et al., “Deformation Field Heterogeneity in Punch Indentation,” Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences, 2014.
50. Dorner, D.; Röller, K.; and Stöckhert, B., “High Temperature Indentation Creep Tests on Anhydrite—A Promising First Look,” Solid Earth, V. 5, No. 2, 2014, pp. 805-819. doi: 10.5194/se-5-805-2014
51. Bastawros, A.-F.; Bart-Smith, H.; and Evans, A. G., “Experimental Analysis of Deformation Mechanisms in a Closed-Cell Aluminum Alloy Foam,” Journal of the Mechanics and Physics of Solids, V. 48, No. 2, 2000, pp. 301-322. doi: 10.1016/S0022-5096(99)00035-6