Abstract:
NEU: An ACI Center of Excellence for Carbon Neutral Concrete introduced its new third-party Validation/Verification Program for the cement and concrete industries. NEU’s Program provides third party validation or verification of the environmental claims of both existing and innovative new products and technologies associated with reduced carbon cement, concrete production, and concrete products following International Organization for Standardization (ISO) standards.




  