Stress-Strain Relations for Concrete Under Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stress-Strain Relations for Concrete Under Cyclic Loading

Author(s): B. P. Sinha, Kurt H. Gerstle and Leonard G. Tulin

Publication: Journal Proceedings

Volume: 61

Issue: 2

Appears on pages(s): 195-212

Keywords:

DOI: 10.14359/7775

Date: 2/1/1964

Abstract:
An experimental investigation into the behavior of plain concrete under cyclic loading is described. Stress-strain curves obtained for concrete cylinders under such loading are presented, and analytical stress-strain relations for cyclic loading are derived. Assuming the property of uniqueness of stress-strain rela-tions, it is shown how the cyclic stress-strain curves can be used to predict the behavior of a concrete fiber subjected to an arbitrary load history (neglecting creep).




  