Abstract:
Prestressed concrete lift slabs have been used successfully, not only as an economical method of construction, but also as a medium to obtain flat slab buildings that have no deflection or camber. The analysis of a flat slab can be extremely complex. The beam method has been developed as an approximate but applicable method of design. By this analysis, slabs may be designed for proper behavior and strength without the use of the more complicated plate theory.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer