Title: State-of-the-Art Report on Parking Structures

Author(s): ACI committee 362

Publication: Journal Proceedings

Volume: 82

Issue: 4

Appears on pages(s): 544-578

Keywords: abrasion; admixtures; air entrainment; aluminum; beams ; bond (concrete to reinforcement); bridges (structures); cathodic protec-tion;chlorides; coatings; columns (supports); concrete construction; concrete durability;

DOI: 10.14359/10368

Date: 7/1/1985

Abstract:
Repeatedly, parking structures have strength, serviceability, and durability problems associated with their unique structural requirements and exposure to the elements. Many parking structures that are exposed to a deicer environment show very early signs of corrosion, scaling due to cyclic freeze-thaw damage, and through-slab water penetration. Special considerations are discussed to address the repeating problems resulting from design, construction, maintenance, and user practices. Methods used to evaluate conditions of existing structures are reviewed as well as the strategies employed for their future use. A breadth of maintenance, repair, and protection methods are discussed.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer