Title: Structural Refractory Concrete

Author(s): Herman G. Protze

Publication: Journal Proceedings

Volume: 53

Issue: 3

Appears on pages(s): 871-888

Keywords: no keywords

DOI: 10.14359/11559

Date: 3/1/1957

Abstract:
Theoretical and practical problems in the construction of jet engine test cell exhaust structures are considered, including the development and use of proper materials, mixtures, equipment, and methods for installation of durable structural refractory lightweight aluminous cement concretes. The author draws from laboratory and field experiences on four projects in recommending current optimum techniques for such work.




  