Development of Low Cost Housing Materials Based on Phosphogypsum and Calcium Sulfoaluminate Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Low Cost Housing Materials Based on Phosphogypsum and Calcium Sulfoaluminate Cement

Author(s): J. Ambroise, C. Angulski da Luz, and J. Pera

Publication: Symposium Paper

Volume: 235

Issue:

Appears on pages(s): 125-136

Keywords: building materials; calcium sulfoaluminate cement; ettringite; hydration; phosphogypsum; water-resistance

DOI: 10.14359/15859

Date: 3/22/2006

Abstract:
Gypsum is a cheap binder but its utilization remains limited due to its bad water resistance. The solutions usually proposed to improve this water resistance consist in adding water repelling agents like organo-polysiloxanes to the mixing water. This paper shows that another solution is to mix calcium sulfoaluminate clinker and gypsum. When hydrating, such mixture becomes water-resistant and gypsum is converted into hydraulic binder. Therefore, it is possible to develop low cost housing materials, mainly based on gypsum. The experimental results show that the quantity of calcium sulfoaluminate clinker necessary to stabilize gypsum is in the range of 20 to 30% of the total amount of binder (phosphogypsum + calcium sulfoaluminate cement). In such case, resistance to wetting-drying cycles is very good. Building materials like concrete blocks, renders, and screeds were developed and behaved very well under natural weathering for more than 18 months. This can be a solution to valorize large amounts of gypsum by-products and develop low cost housing materials.




  