Title: Construction of Reinforced Concrete Factory Building with Submerged Foundations Under Severe Tidal Conditions

Author(s): N.M. Loney

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 133-140

Keywords: none

DOI: 10.14359/15985

Date: 2/1/1916

Abstract:
During the winter of 1914-15, the company of which the author is he enigneer decoded to construct a reinforced concrete factory at Lubee, Me., in order to bettwe protect the industry which it serves from danger of interruption by fire.




  