Stress at Ultimate in Unbonded Post-Tensioning Tendons: Part 1--Evaluation of the State of the Art

International Concrete Abstracts Portal

  


Title: Stress at Ultimate in Unbonded Post-Tensioning Tendons: Part 1--Evaluation of the State of the Art

Author(s): Antoine E. Naaman and Fadi M Alkhairi

Publication: Structural Journal

Volume: 88

Issue: 5

Appears on pages(s): 641-651

Keywords: bond (concrete to reinforcement); post-tensioning; prestressed concrete; prestressing steels; standards; strength; stresses; unbonded prestressing; Structural Research

DOI: 10.14359/2763

Date: 9/1/1991

Abstract:
This study deals with the stress at ultimate ps in unbonded tendons of prestressed and partially prestressed beams for the purpose of computing their nominal bending moment resistance. The first part comprises mainly: 1) some background information followed by a comprehensive review of existing experimental and analytical investigations dealing with the stress at ultimate in unbonded tendons; 2) a summary of prediction equations for fps suggested by different investigators and in various North American and European codes; and 3) an evaluation of typical prediction equations achieved by comparing predicted with experimentally observed results. The experimental results were obtained from nine different investigations totaling 143 beam tests described in the technical literature and carried out since 1960 in various parts of the world. In the second part of this study, the background for a new rational methodology for analysis of beams prestressed with unbonded tendons is covered and a new prediction equation for fps at ultimate is developed. The equation is shown to account for most of the variables found important in the analysis of beams prestressed with unbonded tendons and to predict experimental results with much better accuracy than any of the existing prediction equations reviewed in the first part. The proposed equation modified by an appropriate safety factor is recommended for adoption by the ACI Building Code.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer