Title: Influence of Material Ductility on Performance of Concrete Repair

Author(s): Mo Li and Victor C. Li

Publication: Materials Journal

Volume: 106

Issue: 5

Appears on pages(s): 419-428

Keywords: cracking; ductility; durability; interface delamination; repair; shrinkage; simulation.

DOI: 10.14359/51663142

Date: 9/1/2009

Abstract:
The lack of durability in concrete repairs induces premature repair deterioration. Drying shrinkage of "new" repair material restrained by "old" concrete substrate results in repair layer cracking, and interface delamination between the repair and the concrete substrate. This paper investigates a material solution to these common repair failures. A high-early-strength engineered cementitious composite (HES-ECC) developed for concrete repair is employed for this study. The HES-ECC possesses high early-age strength (over 47 MPa [6885 psi] in 7 days) and high tensile strain capacity several hundred times that of normal concrete or fiberreinforced concrete (FRC). Experimental and numerical studies on a layered repair system were conducted to verify that the high ductility of HES-ECC can relieve shrinkage-induced stresses in the repair layer and at the repair/old concrete interface, thereby simultaneously suppressing large repair surface cracks and interface delamination. Detailed results of these studies are reported in this paper.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer