Title: Interfacial Bond between Reinforcing Fibers and Calcium Sulfoaluminate Cements: Fiber Pullout Characteristics

Author(s): Robert B. Jewell, Kamyar C. Mahboub, Thomas L. Robl, and Arne C. Bathke

Publication: Materials Journal

Volume: 112

Issue: 1

Appears on pages(s): 39-48

Keywords: CSA cement; fibers; interfacial bond; low-energy cement; pullout test

DOI: 10.14359/51687234

Date: 1/1/2015

Abstract:
This paper presents the results of an experimental investigation on the influence of the interfacial bond of reinforcing fibers embedded in a calcium sulfoaluminate matrix on the fiber-pullout peak load and energy consumption. Bonding at the fiber-matrix interface plays an important role in controlling the mechanical performance of cementitious composites—in particular, composites formed from sulfate-based systems (calcium sulfoaluminate cements [CSA]), as opposed to the silicate systems found in portland cement. Various types of fibers were selected, including polyvinyl alcohol (PVA), polypropylene, and copper-coated steel. The fibers were embedded in three different matrixes: two sulfate-based cements including one commercially available CSA cement and a CSA fabricated from coal-combustion by-products. The third matrix was a silicatebased ordinary portland cement (OPC). In this study, the results of the single-fiber pullout test were coupled with scanning electron microscopy (SEM) to examine the interfacial bond between the fiber and CSA matrix for evidence of debonding and possible hydration reaction products.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer