Concrete Q&A: Horizontal Joints in Water Tanks
Author(s):
Charles S. Hanskat
Publication:
Concrete International
Volume:
36
Issue:
10
Appears on pages(s):
99-100
Keywords:
DOI:
Date:
10/1/2014
Abstract:
Q. Are horizontal joints allowed in a concrete water tank wall? If they are, could you refer me to an ACI document containing more details on the subject? I checked ACI 224.3R-951 but found no relevant information.