Title: 
            Compatibility of Superplasticisers in Concrete with Mixed Recycled Aggregate
        
        
            Author(s): 
            C. Medina, W. Zhu, E.Asensio, I.F. Saéz del Bosque, M. Frías, and M. I. Sánchez de Rojas
        
        
            
                Publication: 
                Symposium Paper
            
            
                Volume: 
                303
            
            
                Issue: 
                
            
            
                Appears on pages(s): 
                281-292
            
            
                Keywords: 
                concretes; construction and demolition waste; mixed recycled aggregate/ superplasticisers
            
            
                DOI: 
                10.14359/51688140
            
        
        
            Date: 
            6/1/2015
        
        
            Abstract:
            The use of superplasticisers to enhance concrete properties is standard practice in concrete manufacture. The present study aimed to assess the compatibility of these admixtures with recycled construction and demolition waste (with or without lightweight materials) aggregate on some the physical and mechanical properties of the resulting concrete. The paper reports on the 0 and 50% replacement of natural coarse aggregate in a conventional concrete with mixed recycled coarse aggregate. The experimental technique used was based on the study of water absorption as well as the compressive and splitting tensile strength of such recycled concretes. The superplasticiser was found to be compatible with this type of recycled aggregate, for no decline in concrete performance was observed.