Title: Fatigue Strength of Reinforced Concrete Beams without Links under Shear Loads

Author(s): Guenter Axel Rombach and Matthias Kohl

Publication: Structural Journal

Volume: 113

Issue: 5

Appears on pages(s): 941-950

Keywords: fatigue design; reinforced concrete without shear reinforcement; shear design

DOI: 10.14359/51688924

Date: 9/1/2016

Abstract:
The design of reinforced concrete (RC) structures against fatigue failure due to shear loads is based on empirical approaches (refer to Eurocode 2). In particular, this unsatisfying status pertains to members without links such as bridge slabs or footings of wind energy plants. In terms of sustainability—for example, a longer service life of these structures—safe and exact calculation methods to determine their fatigue resistance are urgently needed. Therefore, the load-bearing behavior of RC elements without links under static and cyclic loads was studied theoretically, experimentally, and numerically at the Hamburg University of Technology (TUHH). Sixteen RC beams without shear reinforcement were tested under cyclic loads. The analysis of the time-consuming experimental investigations confirmed the EC2 approach to estimate the shear capacity of RC beams without links under fatigue loading, if the shear resistance under static loads is known from tests. The fib approach is too conservative. The specimens showed a high shear strength even after wide cracks had opened. Thus, the shear force is predominantly carried by the compression zone and not by crack friction.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer