Relating Formation Factor of Concrete to Water Absorption

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Relating Formation Factor of Concrete to Water Absorption

Author(s): Mehdi Khanzadeh Moradllo, Chunyu Qiao, Burkan Isgor, Steven Reese, and W. Jason Weiss

Publication: Materials Journal

Volume: 115

Issue: 6

Appears on pages(s): 887-898

Keywords: absorption; durability; formation factor; neutron radiography; performance specification; resistivity

DOI: 10.14359/51706844

Date: 11/1/2018

Abstract:
The absorption of fluid in concrete is a key parameter that can be related to many durability-related deterioration mechanisms. The current water absorption testing procedure (ASTM C1585-13) is time-consuming due to both sample conditioning and the test duration. This study examines whether the formation factor can be used to estimate water absorption and thereby greatly reduce the time of testing. This paper describes the use of neutron radiography to examine water absorption in mortar mixtures with varying water-cement ratios (w/c) that have been preconditioned to two different moisture states (relative humidities). Theoretical derivations and experimental results indicate a linear relationship between initial sorptivity and the reciprocal of the square root of the formation factor. The experimental depth of water penetration was compared with a theoretical formulation and the results showed good agreement.

Related References:

1. Weiss, W. J.; Barrett, T. J.; Qiao, C.; and Todak, H., “Toward a Specification for Transport Properties of Concrete Based on the Formation Factor of a Sealed Specimen,” Advances in Civil Engineering Materials, V. 5, No. 1, 2016, pp. 179-194. doi: 10.1520/ACEM20160004

2. Weiss, W. J.; Ley, M. T.; Isgor, O. B.; and Van Dam, T., “Toward Performance Specifications for Concrete Durability: Using the Formation Factor for Corrosion and Critical Saturation for Freeze-Thaw,” Transportation Research Board 96th Annual Meeting, Washington, DC, 2017 20 pp.

3. Weiss, W. J.; Spragg, R. P.; Isgor, O. B.; Ley, M. T.; and Van Dam, T., “Toward Performance Specifications for Concrete: Linking Resistivity, RCPT and Diffusion Predictions Using the Formation Factor for Use in Specifications,” High Tech Concrete: Where Technology and Engineering Meet, Springer, Berlin, Germany, 2018, pp. 2057-2065.

4. Yu, T.; Bognacki, C. J.; Obla, K. H.; Hicks, J. K.; D’Ambrosia, M. D.; and Weiss, W. J.; Fu, T.; and Giannini, E. R., “From Research to Reality, Can We Implement Performance-Based Specifications for Durability and Longevity of Concrete? Will They Work?” Concrete International, V. 39, No. 1, Jan. 2017, pp. 39-46.

5. Rupnow, T., and Icenogle, P., “Surface Resistivity Measurements Evaluated as Alternative to Rapid Chloride Permeability Test for Quality Assurance and Acceptance,” Transportation Research Record: Journal of the Transportation Research Board, V. 2290, No. 1, 2012, pp. 30-37. doi: 10.3141/2290-04

6. Sato, T., and Beaudoin, J., An AC Impedance Spectroscopy Study of Freezing Phenomena in Wollastonite Micro-Fibre Reinforced Cement Paste, Thomas Telford Publishing, London, UK, 2003, pp. 379-388.

7. Sohn, D., and Mason, T. O., “Electrically Induced Microstructural Changes in Portland Cement Pastes,” Advanced Cement Based Materials, V. 7, No. 3-4, 1998, pp. 81-88. doi: 10.1016/S1065-7355(97)00056-4

8. Khanzadeh Moradllo, M.; Sudbrink, B.; Hu, Q.; Aboustait, M.; Tabb, B.; Ley, T.; and Davis, J. M., “Using Micro X-Ray Fluorescence to Image Chloride Profiles in Concrete,” Cement and Concrete Research, V. 92, 2017, pp. 128-141. doi: 10.1016/j.cemconres.2016.11.014

9. Nokken, M., and Hooton, D., “Using Pore Parameters to Estimate Permeability or Conductivity of Concrete,” Materials and Structures, V. 41, No. 1, 2007, pp. 1-16. doi: 10.1617/s11527-006-9212-y

10. Sant, G., and Weiss, J., “Using X-Ray Absorption to Assess Moisture Movement in Cement-Based Materials,” Journal of ASTM International, V. 6, No. 9, 2009, pp. 1-15.

11. Van Belleghem, B.; Montoya, R.; Dewanckele, J.; Van den Steen, N.; De Graeve, I.; Deconinck, J.; Cnudde, V.; Van Tittelboom, K.; and De Belie, N., “Capillary Water Absorption in Cracked and Uncracked Mortar—A Comparison between Experimental Study and Finite Element Analysis,” Construction and Building Materials, V. 110, 2016, pp. 154-162. doi: 10.1016/j.conbuildmat.2016.02.027

12. Khanzadeh Moradllo, M., and Ley, M. T., “Quantitative Measurement of the Influence of Degree of Saturation on Ion Penetration in Cement Paste by Using X-Ray Imaging,” Construction and Building Materials, V. 141, 2017, pp. 113-129. doi: 10.1016/j.conbuildmat.2017.03.007

13. Spragg, R.; Villani, C.; Snyder, K.; Bentz, D.; Bullard, J.; and Weiss, J., “Factors that Influence Electrical Resistivity Measurements in Cementitious Systems,” Transportation Research Record: Journal of the Transportation Research Board, V. 2342, No. 1, 2013, pp. 90-98. doi: 10.3141/2342-11

14. Burden, D., “The Durability of Concrete Containing High Levels of Fly Ash,” MSc thesis, The University of New Brunswick, Fredericton, NB, Canada, 2006, 110 pp.

15. Coyle, A.; Spragg, R.; Amirkhanian, A.; and Weiss, J., “Measuring the Influence of Temperature on Electrical Properties of Concrete,” Service Life of Cement-Based Materials and Structures, RILEM, Lyngby, Denmark, 2016, 211 pp.

16. Spragg, R.; Bu, Y.; Snyder, K.; Bentz, D.; and Weiss, J., “Electrical Testing of Cement-Based Materials: Role of Testing Techniques, Sample Conditioning, and Accelerated Curing,” Publication FHWA/IN/JTRP-2013/28, Joint Transportation Research Program, Indiana Department of Transportation and Purdue University, West Lafayette, IN, 2013.

17. Spragg, R.; Jones, S.; Bu, Y.; Lu, Y.; Bentz, D.; Snyder, K.; and Weiss, J., “Leaching of Conductive Species: Implications to Measurements of Electrical Resistivity,” Cement and Concrete Composites, V. 79, 2017, pp. 94-105. doi: 10.1016/j.cemconcomp.2017.02.003

18. Archie, G. E., “The Electrical Resistivity Log as an Aid in Determining Some Reservoir Characteristics,” Transactions of the AIME, V. 146, No. 1, 1942, pp. 54-62.

19. Adamson, A., and Gast, A. P., Physical Chemistry of Surfaces, Wiley Interscience, New York, 1997, 808 pp.

20. Dean, J., “Lange’s Handbook of Chemistry,” Materials and Manufacturing Processes, V. 5, No. 4, 1990, pp. 687-688. doi: 10.1080/10426919008953291

21. Katz, A., and Thompson, A., “Quantitative Prediction of Permeability in Porous Rock,” Physical Review B, V. 34, No. 11, 1986, pp. 8179-8181. doi: 10.1103/PhysRevB.34.8179

22. Castro, J.; Bentz, D.; and Weiss, J., “Effect of Sample Conditioning on the Water Absorption of Concrete,” Cement and Concrete Composites, V. 33, No. 8, 2011, pp. 805-813. doi: 10.1016/j.cemconcomp.2011.05.007

23. Hall, C., and Hoff, W. D., Water Transport in Brick, Stone and Concrete, Spon Press, Taylor & Francis Group, New York, 2002.

24. Sears, V. F., “Neutron Scattering Lengths and Cross Sections,” Neutron News, V. 3, No. 3. 1992, pp. 26-37.

25. Rajabipour, F., “In-situ Electrical Sensing and Material Health Monitoring in Concrete Structures,” PhD thesis, Purdue University, West Lafayette, IN, 2006, 173 pp.

26. Spragg, R. P., “The Rapid Assessment of Transport Properties of Cementitious Materials Using Electrical Methods,” MSc thesis, Purdue University, West Lafayette, IN, 2013, 186 pp.

27. Kelham, S., “A Water Absorption Test for Concrete,” Magazine of Concrete Research, V. 40, No. 143, 1988, pp. 106-110. doi: 10.1680/macr.1988.40.143.106

28. Christensen, B. J.; Mason, T. O.; and Jennings, H. M., “Comparison of Measured and Calculated Permeabilities for Hardened Cement Pastes,” Cement and Concrete Research, V. 26, No. 9, 1996, pp. 1325-1334. doi: 10.1016/0008-8846(96)00130-5

29. Tumidajski, P., and Lin, B., “On the Validity of the Katz-Thompson Equation for Permeabilities in Concrete,” Cement and Concrete Research, V. 28, No. 5, 1998, pp. 643-647. doi: 10.1016/S0008-8846(98)00032-5

30. Bu, Y.; Spragg, R.; and Weiss, W., “Comparison of the Pore Volume in Concrete as Determined Using ASTM C642 and Vacuum Saturation,” Advances in Civil Engineering Materials, V. 3, No. 1, 2014, pp. 308-315. doi: 10.1520/ACEM20130090

31. Snyder, K. A.; Feng, X.; Keen, B.; and Mason, T., “Estimating the Electrical Conductivity of Cement Paste Pore Solutions from OH–, K+ and Na+ Concentrations,” Cement and Concrete Research, V. 33, No. 6, 2003, pp. 793-798. doi: 10.1016/S0008-8846(02)01068-2

32. Bentz, D. P., “A Virtual Rapid Chloride Permeability Test,” Cement and Concrete Composites, V. 29, No. 10, 2007, pp. 723-731. doi: 10.1016/j.cemconcomp.2007.06.006

33. Bu, Y., and Weiss, J., “The Influence of Alkali Content on the Electrical Resistivity and Transport Properties of Cementitious Materials,” Cement and Concrete Composites, V. 51, 2014, pp. 49-58. doi: 10.1016/j.cemconcomp.2014.02.008

34. Weiss, J.; Snyder, K.; Bullard, J.; and Bentz, D., “Using a Saturation Function to Interpret the Electrical Properties of Partially Saturated Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 8, 2013, pp. 1097-1106. doi: 10.1061/(ASCE)MT.1943-5533.0000549

35. Snyder, K. A.; Ferraris, C.; Martys, N.; and Garboczi, E. J., “Using Impedance Spectroscopy to Assess the Viability of the Rapid Chloride Test for Determining Concrete Conductivity,” Journal of Research of the National Institute of Standards and Technology, V. 105, No. 4, 2000, pp. 497-509. doi: 10.6028/jres.105.040

36. Hickner, M.; Siegel, N.; Chen, K.; Hussey, D.; Jacobson, D.; and Arif, M., “In Situ High-Resolution Neutron Radiography of Cross-Sectional Liquid Water Profiles in Proton Exchange Membrane Fuel Cells,” Journal of the Electrochemical Society, V. 155, No. 4, 2008, pp. B427-B34. doi: 10.1149/1.2826287

37. Hussey, D.; Spernjak, D.; Weber, A.; Mukundan, R.; Fairweather, J.; Brosha, E.; Davey, J.; Spendelow, J. S.; Jacobson, D. L.; and Borup, R. L., “Accurate Measurement of the Through-Plane Water Content of Proton-Exchange Membranes Using Neutron Radiography,” Journal of Applied Physics, V. 112, No. 10, 2012, p. 104906 doi: 10.1063/1.4767118

38. Lucero, C.; Spragg, R.; Bentz, D.; Hussey, D.; Jacobson, D.; and Weiss, J., “Neutron Radiography Measurement of Salt Solution Absorption in Mortar,” ACI Materials Journal, V. 114, No. 1, Jan.-Feb. 2017, pp. 149-159. doi: 10.14359/51689488

39. Schneider, C. A.; Rasband, W. S.; and Eliceiri, K. W., “NIH Image to ImageJ: 25 Years of Image Analysis,” Nature Methods, V. 9, No. 7, 2012, pp. 671-675. doi: 10.1038/nmeth.2089

40. Kang, M.; Bilheux, H.; Voisin, S.; Cheng, C.; Perfect, E.; Horita, J.; and Warren, J. M., “Water Calibration Measurements for Neutron Radiography: Application to Water Content Quantification in Porous Media,” Nuclear Instruments & Methods in Physics Research. Section A, Accelerators, Spectrometers, Detectors and Associated Equipment, V. 708, 2013, pp. 24-31. doi: 10.1016/j.nima.2012.12.112

41. Powers, T. C.; Copeland, L. E.; and Mann, H., “Capillary Continuity or Discontinuity in Cement Pastes,” Journal of PCA Research and Development Laboratories, 1959, pp. 38-48.

42. Radlinska, A.; Rajabipour, F.; Bucher, B.; Henkensiefken, R.; Sant, G.; and Weiss, J., “Shrinkage Mitigation Strategies in Cementitious Systems: A Closer Look at Differences in Sealed and Unsealed Behavior,” Transportation Research Record: Journal of the Transportation Research Board, V. 2070, No. 1, 2008, pp. 59-67. doi: 10.3141/2070-08

43. Andrade, C.; Sarría, J.; and Alonso, C., “Relative Humidity in the Interior of Concrete Exposed to Natural and Artificial Weathering,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1249-1259. doi: 10.1016/S0008-8846(99)00123-4

44. Grasley, Z. C.; Lange, D. A.; D’Ambrosia, M. D.; and Villalobos-Chapa, S., “Relative Humidity in Concrete,” Concrete International, V. 28, No. 10, Oct. 2006, pp. 51-57.


ALSO AVAILABLE IN:

Electronic Materials Journal