Title: Does the Size Effect Exist in Reinforced Masonry?

Author(s): Salah R. Sarhat and Edward G. Sherwood

Publication: Symposium Paper

Volume: 328

Issue:

Appears on pages(s): 5.1-5.18

Keywords: Beams, Masonry; Shear Strength, Size Effect

DOI: 10.14359/51711149

Date: 9/12/2018

Abstract:
The research described in this paper studies the effect of the effective depth, d, on the shear behavior of large reinforced masonry beams. Five fully grouted shear critical reinforced masonry beams ranging in effective depth from 300 mm to 1400 mm were tested to failure under three point loading to investigate their cracking behavior and ultimate shear strengths. The experimental shear strengths were compared with the failure shear stresses predicted using three different design codes: the TMS 402 code, the CSA S304.1-2004 code and the CSA A23.3-14 code for reinforced concrete. The test results show that the size effect in reinforced masonry is real and very significant, in that failure shear stresses decreased as the effective depth increased. It is shown that as the effective depth increases, the longitudinal crack width and spacing at mid-depth increase as well. These wider cracks initiate shear failure at a lower shear stress due to reduced aggregate interlock capacity. It is shown that the TMS masonry design code gives non-conservative predictions of the shear strength of large masonry beams. The most accurate prediction of the size effect in masonry is given by the CSA A23.3 -2014 code which is based on the General Method of shear design used extensively to design reinforced concrete. The paper highlights the necessity to revise masonry design codes to address the size effect.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer