Constructability of Post-Tensioning Anchors in Shear Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Constructability of Post-Tensioning Anchors in Shear Walls

Author(s): Phil Diekemper, Frank Salzano, and Bruce Suprenant

Publication: Concrete International

Volume: 40

Issue: 12

Appears on pages(s): 35-37

Keywords: slab, form, tendons, stressing

DOI:

Date: 12/1/2018

Abstract:
Many post-tensioned buildings and parking garages are constructed with unbonded single strand tendons. When the strands terminate near or pass through a structural wall (shear wall), constructability is affected. Congested reinforcement in structural walls, especially in buildings constructed in seismic regions, impedes the placement of anchors and associated reinforcement. In addition, placement of anchorage within walls may make it impossible to use climbing forms to construct walls in advance of floors.




  