Pervious Concrete Production using Recycled Waste Latex Paint

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pervious Concrete Production using Recycled Waste Latex Paint

Author(s): A. Said and O. Quiroz

Publication: Symposium Paper

Volume: 334

Issue:

Appears on pages(s): 205-218

Keywords: Waste latex paint; Latex-modified concrete; Pervious concrete; Durability; Hydraulic properties

DOI: 10.14359/51720264

Date: 9/30/2019

Abstract:
In the U.S. and around the world, large amounts of waste latex paint are generated annually, which creates a significant challenge in terms of disposal in an economic manner. Paint contains some chemicals that may be harmful to the environment if recycled as it contains volatile organic compounds. However, waste latex paint can be used to produce an economic latex-modified pervious concrete that is similar or superior to regular pervious concrete. Previous studies investigated recycling waste latex paint in concrete applications such as sidewalks. This study investigates the use of waste latex paint in producing pervious concrete and the effect of using different ratios of paint addition on the properties of the studied mixtures. The properties evaluated included physical, mechanical and hydraulic properties. Results show that while waste latex paint recycling in pervious concrete can slightly reduce its mechanical properties at 5% polymer to cement content, it can still be a viable option to prevent paint disposal in landfills.




  