International Concrete Abstracts Portal

  


Title: Suitability of Metakaolin-Based Geopolymers for Masonry Plastering

Author(s): Joseph J. Assaad and Marianne Saba

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 269-279

Keywords: geopolymers; masonry cements; metakaolin; plasters; rheology; strength

DOI: 10.14359/51725991

Date: 11/1/2020

Abstract:
The development and use of geopolymers (GP) considerably increased in the construction industry. This paper assesses the suitability of metakaolin-based GP mortars for masonry plastering works, including their comparison to masonry cement (MC) mortars and compliance to relevant EN 413-1 and ASTM C91 specifications. Three classes of GP mortars prepared with different metakaolin-to-limestone ratios are tested; the sodium hydroxide and sodium silicate activators contained air-entraining molecules to secure approximately 10% ±2% air content. Test results showed that GP mortars exhibited excellent water retention and increased rheological properties, which was related to higher viscosity of alkaline solution that increases stickiness and overall cohesiveness. For given limestone concentration, the mechanical properties of GP mortars including the pulloff bond strength and sorptivity were remarkably better than MC mixtures. Almost 90% of ultimate compressive strength was achieved after 7 days for GP mortars cured at ambient temperature, while this varied from 55 to 80% for MC mixtures cured in moist conditions. This can be particularly advantageous in masonry applications to speed up construction operations while, at the same time, eliminate the hassle of moist curing normally required with cement-based plasters.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.