Stiffness Degradation of Concrete Due to Alkali-Silica Reaction: A Computational Homogenization Approach

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stiffness Degradation of Concrete Due to Alkali-Silica Reaction: A Computational Homogenization Approach

Author(s): Thuc Nhu Nguyen, R. Emre Erkmen, Leandro F. M. Sanchez, and Jianchun Li

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 65-76

Keywords: alkali-silica reaction; computational homogenization; crack configuration; representative volume element

DOI: 10.14359/51728125

Date: 11/1/2020

Abstract:
Alkali-silica reaction (ASR) is one of the most harmful distress mechanisms affecting concrete infrastructure worldwide. ASR is a chemical reaction that generates a secondary product, which induces expansive pressure within the reacting aggregate material and adjacent cement paste upon moisture uptake, leading to cracking, loss of material integrity, and functionality of the affected structure. In this work, a computational homogenization approach is proposed to model the impact of ASR-induced cracking on concrete stiffness as a function of its development. A representative volume element (RVE) of the material at the mesoscale is developed, which enables the input of the cracking pattern and extent observed from a series of experimental testing. The model is appraised on concrete mixtures presenting different mechanical properties and incorporating reactive coarse aggregates. The results have been compared with experimental results reported in the literature. The case studies considered for the analysis show that stiffness reduction of ASR-affected concrete presenting distinct damage degrees can be captured using the proposed mesoscale model as the predictions of the proposed methodology fall in between the upper and lower bounds of the experimental results.

Related References:

1. Giaccio, G.; Zerbino, R.; Ponce, J. M.; and Batic, O. R., “Mechanical Behavior of Concretes Damaged by Alkali-Silica Reaction,” Cement and Concrete Research, V. 38, No. 7, 2008, pp. 993-1004. doi: 10.1016/j.cemconres.2008.02.009

2. Multon, S.; Seignol, J. F.; and Toutlemonde, F., “Structural Behavior of Concrete Beams Affected by Alkali-Silica Reaction,” ACI Materials Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 67-76.

3. Swamy, R. N., and Al-Asali, M. M., “Engineering Properties of Concrete Affected by Alkali-Silica Reaction,” ACI Materials Journal, V. 85, No. 5, Sept.-Oct. 1988, pp. 367-374.

4. Fournier, B., and Bérubé, A., “Alkali-Aggregate Reaction in Concrete: A Review of Basic Concepts and Engineering Implications,” Canadian Journal of Civil Engineering, V. 27, No. 2, 2000, pp. 167-191. doi: 10.1139/l99-072

5. Sanchez, L. F. M., “Contribution to the Assessment of Aging Concrete Infrastructures Affected by Alkali-Aggregate Reaction,” PhD thesis, Université Laval, Quebec, QC, Canada, 2014.

6. CSA A23.1, “Concrete Materials and Methods of Concrete Construction—Appendix B,” Canadian Standards Association, Mississauga, ON, Canada, 2014.

7. ASTM C1293-08, “Standard Test Method for Determination of Length Change of Concrete due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

8. Thomas, M. D. A.; Fournier, B.; and Folliard, K. J., “Report on Determining the Reactivity of Concrete Aggregates and Selecting Appropriate Measures for Preventing Deleterious Expansion in New Concrete Construction,” FHWA-HIF-09-001, FHWA & AASHTO ASR Task Group, Washington, DC, 2010.

9. Folliard, K. J.; Barborak, R.; Drimalas, T.; Du, L.; Garber, S.; Ideker, J.; Ley, T.; Williams, S.; and Juenger, M., Fournier, B.; and Thomas,  M. D. A., “Preventing ASR/DEF in New Concrete: Final Report,” FHWA/TX-06/0-4085-5, Texas Department of Transportation, Austin, TX, 2006.

10. Malvar, L. J.; Cline, G. D.; Burke, D. F.; Rollings, R.; Sherman, T.; and Greene, J., “Alkali-Silica Reaction Mitigation: State-of-the-Art,” TR-2195-SHR, Naval Facilities Engineering Service Center, Port Hueneme, CA, 2001.

11. Ballard, Z. J.; Caires, W. S.; and Peters, S. R., “Alternate Mitigation Materials for Alkali-Silica Reaction (ASR) in Concrete,” CDOT-2008-10, Colorado Department of Transportation, DTD Applied Research and Innovation Branch, Denver, CO, 2008.

12. Pietruszczak, S., “On the Mechanical Behaviour of Concrete Subjected to Alkali-Aggregate Reaction,” Computers & Structures, V. 58, No. 6, 1996, pp. 1093-1097. doi: 10.1016/0045-7949(95)00228-6

13. Saouma, V. E., Numerical Modelling of AAR, CRC Press, Boca Raton, FL, 2014.

14. Erkmen, R. E.; Gowripalan, N.; and Sirivivatnanon, V., “Elasto-Plastic Damage Modelling of Beams and Columns with Mechanical Degradation,” Computers and Concrete, V. 19, No. 3, 2017, pp. 315-323. doi: 10.12989/cac.2017.19.3.315

15. Gorga, R.; Sanchez, L.; and Martin-Perez, B., “FE Approach to Perform the Condition Assessment of a Concrete Overpass Damaged by ASR after 50 Years in Service,” Engineering Structures, V. 177, Dec, 2018, pp. 133-146. doi: 10.1016/j.engstruct.2018.09.043

16. Reinhardt, H. W., and Mielich, O., “A Fracture Mechanics Approach to the Crack Formation in Alkali-Sensitive Grains,” Cement and Concrete Research, V. 41, No. 3, 2011, pp. 255-262. doi: 10.1016/j.cemconres.2010.11.008

17. Multon, S.; Sellier, A.; and Cyr, M., “Chemo–Mechanical Modeling for Prediction of Alkali Silica Reaction (ASR) Expansion,” Cement and Concrete Research, V. 39, No. 6, 2009, pp. 490-500. doi: 10.1016/j.cemconres.2009.03.007

18. Poyet, S.; Sellier, A.; Capra, B.; Foray, G.; Torrenti, J. M.; Cognon, H.; and Bourdarot, E., “Chemical Modelling of Alkali Silica Reaction: Influence of the Reactive Aggregate Size Distribution,” Materials and Structures, V. 40, No. 2, 2007, pp. 229-239. doi: 10.1617/s11527-006-9139-3

19. Suwito, A.; Jin, W.; Xi, Y.; and Meyer, C., “A Mathematical Model for the Pessimum Size Effect of ASR in Concrete,” Concrete Science and Engineering, V. 4, No. 13, 2002, pp. 23-34.

20. Nielsen, A.; Gottfredsen, F.; and Thogersen, F., “Development of Stresses in Concrete Structures with Alkali–Silica Reactions,” Materials and Structures, V. 26, No. 3, 1993, pp. 152-158. doi: 10.1007/BF02472932

21. Dunant, C. F., and Scrivener, K. L., “Micro-Mechanical Modelling of Alkali-Silica-Reaction-Induced Degradation Using the AMIE Framework,” Cement and Concrete Research, V. 40, No. 4, 2010, pp. 517-525. doi: 10.1016/j.cemconres.2009.07.024

22. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; Bedoya, M. A. B.; Bastien, J.; and Duchesne, J., “Use of Damage Rating Index to Quantify Alkali-Silica Reaction Damage in Concrete: Fine versus Coarse Aggregate,” ACI Materials Journal, V. 113, No. 4, July-Aug. 2016, pp. 395-407. doi: 10.14359/51688983

23. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; and Duchesne, J., “Reliable Quantification of AAR Damage through Assessment of the Damage Rating Index (DRI),” Cement and Concrete Research, V. 67, Jan, 2015, pp. 74-92. doi: 10.1016/j.cemconres.2014.08.002

24. Comby-Peyrot, I.; Bernard, F.; Bouchard, P. O.; Bay, F.; and Garcia-Diaz, E., “Development and Validation of a 3D Computational Tool to Describe Concrete Behaviour at Mesoscale. Application to the Alkali-Silica Reaction,” Computational Materials Science, V. 46, No. 4, 2009, pp. 1163-1177. doi: 10.1016/j.commatsci.2009.06.002

25. Cusatis, G.; Di Luzio, G.; and Cedolin, L., “Meso-Scale Simulation of Concrete: Blast and Penetration Effects and AAR Degradation,” Applied Mechanics and Materials, V. 82, July, 2011, pp. 75-80. doi: 10.4028/www.scientific.net/AMM.82.75

26. Iskhakov, T.; Timothy, J. J.; and Meschke, G., “Expansion and Deterioration of Concrete due to ASR: Micromechanical Modeling and Analysis,” Cement and Concrete Research, V. 115, Jan, 2019, pp. 507-518. doi: 10.1016/j.cemconres.2018.08.001

27. Rezakhani, R.; Alnaggar, M.; and Cusatis, G., “Multiscale Homogenization Analysis of Alkali-Silica Reaction (ASR) Effect in Concrete,” Engineering, V. 5, No. 6, 2019, pp. 1139-1154. doi: 10.1016/j.eng.2019.02.007

28. Holmes, M. H., Introduction to Perturbation Methods, second edition, Springer, New York, 2013.

29. Kanit, T.; Forest, S.; Galliet, I.; Mounoury, V.; and Jeulin, D., “Determination of the Size of the Representative Volume Element for Random Composites: Statistical and Numerical Approach,” International Journal of Solids and Structures, V. 40, No. 13-14, 2003, pp. 3647-3679. doi: 10.1016/S0020-7683(03)00143-4

30. Miehe, C., and Koch, A., “Computational Micro-to-Macro Transitions of Discretized Microstructures Undergoing Small Strains,” Archive of Applied Mechanics, V. 72, No. 4-5, 2002, pp. 300-317. doi: 10.1007/s00419-002-0212-2

31. Belytschko, T.; Liu, W. K.; Moran, B.; and Elkhodary, K., Nonlinear Finite Elements for Continua and Structures, Wiley & Sons, West Sussex, UK, 2014.

32. Larsson, F; Runesson, K.; Saroukhani, S.; and Vafadari, R., “Computational Homogenization Based on a Weak Format of Micro-Periodicity for RVE-Problems,” Computer Methods in Applied Mechanics and Engineering, V. 200, No. 1-4, 2011, pp. 11-26. doi: 10.1016/j.cma.2010.06.023

33. Melenk, J. M., and Babuška, I., “The Partition of Unity Finite Element Method: Basic Theory and Applications,” Computer Methods in Applied Mechanics and Engineering, V. 139, No. 1-4, 1996, pp. 289-314. doi: 10.1016/S0045-7825(96)01087-0

34. Belytschko, T., and Black, N., “Elastic Crack Growth in Finite Elements with Minimal Remeshing,” International Journal for Numerical Methods in Engineering, V. 45, No. 5, 1999, pp. 601-620. doi: 10.1002/(SICI)1097-0207(19990620)45:53.0.CO;2-S

35. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; Mitchell, D.; and Bastien, J., “Overall Assessment of Alkali-Aggregate Reaction (AAR) in Concretes Presenting Different Strengths and Incorporating a Wide Range of Reactive Aggregate Types and Natures,” Cement and Concrete Research, V. 93, Mar. 2017, pp. 17-31. doi: 10.1016/j.cemconres.2016.12.001

36. Wriggers, P., and Moftah, S. O., “Mesoscale Models for Concrete: Homogenisation and Damage Behaviour,” Finite Elements in Analysis and Design, V. 42, No. 7, 2006, pp. 623-636. doi: 10.1016/j.finel.2005.11.008

37. Kim, S.-M., and Abu Al-Rub, R. K., “Meso-Scale Computational Modeling of the Plastic-Damage Response of Cementitious Composites,” Cement and Concrete Research, V. 41, No. 3, 2011, pp. 339-358. doi: 10.1016/j.cemconres.2010.12.002

38. Mirkhalaf, S. M.; Andrade Pires, F. M.; and Simoes, R., “Determination of the Size of the Representative Volume Element for the Simulation of Heterogeneous Polymers at Finite Strains,” Finite Elements in Analysis and Design, V. 119, Oct, 2016, pp. 30-44. doi: 10.1016/j.finel.2016.05.004

39. Rezakhani, R.; Zhou, X.; and Cusatis, G., “Adaptive Multiscale Homogenization of the Lattice Discrete Particle Model for the Analysis of Damage and Fracture in Concrete,” International Journal of Solids and Structures, V. 125, Oct, 2017, pp. 50-67. doi: 10.1016/j.ijsolstr.2017.07.016

40. Sukumar, N.; Chopp, D. L.; Moes, N.; and Belytschko, T. C., ��Modeling Holes and Inclusions by Level Sets in the Extended Finite-Element Method,” Computer Methods in Applied Mechanics and Engineering, V. 190, No. 46-47, 2001, pp. 6183-6200. doi: 10.1016/S0045-7825(01)00215-8


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer