Abstract:
A significant body of research is available on the strength of steel fibre reinforced concrete (SFRC) members subjected to shear and flexure. The behaviour of SFRC under service loads has received less research attention. As the fibres are capable of transmitting tensile stress across a crack, the average tensile strain at a crack in a reinforced concrete member containing fibres is less than that in a similar member without fibres. As a result, the cracking and deformation characteristics of reinforced concrete structures can be significantly improved by adding fibres to the concrete mix. This paper first describes a physically rationale model of the tension stiffening behaviour of SFRC. With this behaviour quantified, expressions suitable for the design of SFRC members are derived for the control of instantaneous deflections and crack widths. Finally, a short example is provided.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer