Title:
346-90/346R-90: Standard Specification for Cast-in-Place Nonreinforced Concrete Pipe & Recommendations for Cast-in-Place Nonreinforced Concrete Pipe
Author(s):
Publication:
Technical Documents
Volume:
Issue:
Appears on pages(s):
22
Keywords:
pipelines
DOI:
Date:
5/1/1990
Abstract:
Note: A newer version of this document exists. This document was replaced by 346-01.
These specifications cover construction of cast-in-place nonreinforced concrete pipe used for the conveyance of liquids such as irrigation water, storm water, sewerage, and industrial wastes. The specifications are a reference standard which the engineer or architect may make applicable to any cast-in-place type project by citing them in the project specifications. The second part of the bulletin presents a general view of present knowledge together with recommendations for design, construction, and testing procedures.