Abstract:
This study presents an analytical model for estimating the effective compressive strength of a reinforced concrete (RC) column intersected by a floor slab made of relatively low-grade concrete. The proposed model is based on a theoretically sound background and considers the force equilibrium and strain compatibility conditions in the vicinity of the interface between the upper and lower columns and an intervening slab. By using the parametric study results obtained from finite element analyses, the effects of the confinement provided by the surrounding slab and the secondary stresses induced by the Poisson effect in the columns and slab panel zone were formulated in detail. A simple design expression was then derived for the better applicability of the proposed method for the estimation of the effective compressive strength of the exterior and interior columns with an intervening slab, in a unified manner. To verify the proposed model, the test results of 81 exterior columns and 24 interior columns were collected from the literature. It was found that the effective compressive strengths obtained by the proposed methods were in good agreement with these test results.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer