Nanotechnology for Improved Three-Dimensional Concrete Printing Constructability

International Concrete Abstracts Portal

  


Title: Nanotechnology for Improved Three-Dimensional Concrete Printing Constructability

Author(s): J. Kruger, S. Cho, M. van den Heever, F. Bester, A. van Rooyen, and G. van Zijl

Publication: Materials Journal

Volume: 118

Issue: 6

Appears on pages(s): 19-28

Keywords: buildability; high-performance concrete (HPC); interlayer bond strength; lightweight foamed concrete (LWFC); mechanical properties; nanoparticles; rheology; thixotropy; three-dimensional (3D) concrete printing

DOI: 10.14359/51733101

Date: 11/1/2021

Abstract:
This paper investigates the application of nanotechnology in three-dimensional (3D) concrete printing (3DCP), in particular for enhancing thixotropic material behavior, improving buildability or the vertical building rate, and the amelioration of typical 3DCP anisotropic mechanical properties. Two 3D-printable cementitious materials are investigated in this study: 1) high-performance concrete (HPC) with respective nano-silica (nS) and silicon carbide (SiC) nanoparticle additions; and 2) lightweight foamed concrete (LWFC) with nS addition. The results indicate a significant increase in thixotropic material behavior for the HPC at low nanoparticle dosages. The inclusion of SiC nanoparticles improved the HPC’s buildability performance by 45%. The incorporation of 3% nS to the LWFC increased the static yield shear stress by up to five times, which is validated by the improved buildability performance. Hardened state mechanical properties improved for both cementitious materials and nanoparticle additions. Especially noteworthy is nanoparticles’ favorable influence on the interlayer bond strength.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer