Title: Concrete Q&A: Synthetic Air-Entraining Admixtures and Air Content Requirements/Recommendations

Author(s): Michael A. Caldarone, Lawrence R. Roberts, and Emmanuel K. Attiogbe

Publication: Concrete International

Volume: 43

Issue: 12

Appears on pages(s): 71-72

Keywords:

DOI:

Date: 12/1/2021

Abstract:
Q. I recently conducted an extensive review of concrete industry standards for requirements and recommendations for air contents specified for freezing-and-thawing durability. Unfortunately, my review shows that the requirements/recommendations included in ACI documents and ASTM standards do not reflect the use of synthetic air-entraining admixtures (AEAs). Rather, these requirements/recommendations are based on concrete mixtures prepared using neutralized vinsol resin AEA, which creates a different air-void system than synthetic AEAs. How can I adjust air content requirements in my specifications to accommodate the use of synthetic AEAs and still meet the requirements/recommendations included in ACI and ASTM documents?




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer