Title: Pyrrhotite in Concrete Aggregates

Author(s): Anthony F. Bentivegna, April Snyder, and Stephen M. Stacey

Publication: Concrete International

Volume: 45

Issue: 8

Appears on pages(s): 37-44

Keywords: mineral, sulfide, deterioration, reaction

DOI:

Date: 8/1/2023

Abstract:
Concrete aggregates produced in two regions in North America have been identified as the cause of deterioration to tens of thousands of residential and light commercial concrete foundations. The article provides an overview of the deterioration mechanism, manifestations of the reaction in North America, current state of knowledge for identification and quantification, and current and proposed legislation.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer