Riverworks at Eastern Wharf is a mixed-use development in Savannah, GA, USA. A massive fire at the construction site caused severe damage to this project. The article describes the investigation of the structure’s condition after the fire, damage evaluation, and repair of the concrete structure of the podium slab and post-tensioning cables.




  