Title: Vertical Punching Capacity of Reinforced Concrete Flat Plates without Shear Reinforcement

Author(s): Srinivas Mogili, Hsiang-Yun Lin, and Shyh-Jiann Hwang

Publication: Structural Journal

Volume: 121

Issue: 1

Appears on pages(s): 171-184

Keywords: ACI 318; analytical model; design codes; Eurocode 2; flat plates; punching; reinforced concrete; shear strength; softened strut-and-tie (SST)

DOI: 10.14359/51739193

Date: 1/1/2024

Abstract:
Reinforced concrete flat-plate systems are widely adopted in buildings owing to ease of construction and facilitating larger clear story heights. Flat plates are routinely designed for two-way shear to preclude brittle punching failures. Accurate assessment of concrete contribution to shear strength is particularly important for flat plates in carrying out a reliable and economical design. To address this, an efficient analytical method based on the softened strut-and-tie model to estimate punching capacity of flat plates without shear reinforcement under gravity loading is presented. The proposed method can account for the influence of various key parameters such as concrete strength, plate thickness, column geometry, longitudinal reinforcement area, and arrangement of tension reinforcement. The proposed method, when verified against data from 224 specimens reported in the literature, showed reasonably good accuracy with a mean test-to-estimated capacity ratio of 1.20 and a coefficient of variation (CoV) of 0.19. In comparison, average capacity ratios using ACI 318-19 and Eurocode 2 provisions were 1.60 and 1.27 (CoV of 0.34 and 0.29), respectively. A comprehensive discussion on the effects of key parameters on punching behavior of flat plates without shear reinforcement is presented, and suggestions to improve existing design provisions are provided.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer