Title: The Intersection of Socially Engaged Art, Concrete, and Climate Action

Author(s): Adam Roberti, Xavier Cortada, and Francisco De Caso

Publication: Concrete International

Volume: 46

Issue: 3

Appears on pages(s): 43-46

Keywords: sculpture, sea, level, park

DOI:

Date: 3/1/2024

Abstract:
A permanent interactive art installation of sustainable concrete elevation sculptures ("The Underwater") is being created across all parks in Miami-Dade County, FL, USA. The installation was initiated by the local artist Xavier Cortada as an art project to create yard signs and painted street intersections that bring attention to the area's vulnerability to rising sea levels.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer