Title: Readily Implementable Sustainable Solutions for Pavement Concretes: Agency and Industry Perspective

Author(s): Michelle A. Helsel, Milena Rangelov, Robert Spragg, Michael Praul

Publication: Symposium Paper

Volume: 361

Issue:

Appears on pages(s): 16-30

Keywords: sustainability, embodied carbon, LCA, concrete pavements, environmental impacts, greenhouse gases, climate change

DOI: 10.14359/51740604

Date: 3/1/2024

Abstract:
To support a rapid integration of sustainability principles into paving concrete practice, this study provides a closer look into readily implementable cement and concrete decarbonization strategies. To do so, this study relies on combined stakeholder involvement, quantitative analysis using Life Cycle Assessment (LCA), and the state-of-the-practice in the US paving concrete industry to understand merits of each solution. The results indicate that concrete mix design optimization is a promising, yet not widely applied solution that can reduce costs, enhance durability, and provide average carbon emissions savings of 14 percent. Use of supplementary cementitious materials (SCM) is another solution with multiple benefits, however, the use of SCM is already widely implemented across the USA. Industry-wide improvement in cement carbon footprint due to energy efficiency can provide additional savings of up to 10 percent. Quantifying the environmental footprint of concrete is critical to inform decision-making and enable more sustainable outcomes.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer