Title:
Review and Analysis of FRP Bond Lengths from Pull-out Testing Database with Reduced Embedment Lengths
Author(s):
John J. Myers
Publication:
Symposium Paper
Volume:
360
Issue:
Appears on pages(s):
21-35
Keywords:
Bond performance; Bond strength; Embedment length; Pull-out test; Rebar diameter; Rebar type.
DOI:
10.14359/51740614
Date:
3/1/2024
Abstract:
The American Concrete Institute (ACI) 440.1R-15 Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars linearly reduces the bar stress and thereby pull-out capacity of FRP bars to zero from an embedment length at 20 bar diameters (db) or less. Most experimental research and data examine the development length of various FRP bars at longer, more traditional, embedment lengths. A database was created from select available data in literature to compare to empirical standards. This investigation examines the bond performance of short embedded FRP bars into concrete considering a pull-out failure mode to expand the understanding of short embedded FRP bars into concrete. Based upon the database collected, for the glass fiber-reinforced polymer (GFRP) rebars, the current 440.1R appear quite conservative. For the basalt fiber-reinforced polymer (BFRP) rebar database collected, the current ACI 440.1R-15 provisions appear unconservative for a statistically significant number of the specimen test results within the database. In the case of the carbon fiber-reinforced polymer (CFRP) database, which is quite limited, the data appears to develop considerably less bond strength than the current 440.1R provisions might suggest which requires deeper investigation for the case of short embedment length bonded CFRP bars.