Title: Cracks Development, Brittle Failure, and Design of Concrete Elements

Author(s): Vitalii Mitrofanov and Pavel Mytrofanov

Publication: Structural Journal

Volume: 122

Issue: 2

Appears on pages(s): 49-58

Keywords: concrete elements brittle failure; critical crack length; fracture process zone (FPZ); rupture crack; strength design

DOI: 10.14359/51743293

Date: 3/1/2025

Abstract:
The limitations of known fracture mechanics (FM) models are noted, and to overcome them, a specific FM model was proposed based on modeling the stress distribution only along the crack fracture process zone (FPZ), with elastic concrete behavior out of the FPZ. This peculiar stress distribution was called physically verisimilar stress (PVS), and it was accepted as the basis of the proposed PVS model, which used three material parameters: maximum stress, intrastructural linear size a, and dimensionless value n, taking into account the plastic properties of the material. The relationships for determining the PVS model parameters were suggested for concrete. Strength problems were solved by the modified method of sections, in which the PVS was applied along the FPZ. The FM model based on PVS and the modified method of sections led to an acceptable in-practice method of strength design, which was considerably simpler than the known phase-field method. The proposed PVS model and design method allow for the prediction of the cracks development, considering their stable growth up to the critical (ultimate) values of the crack length and load. The unstable cracks propagation is considered also. The paper provides examples of designs and shows sufficient theoretical strength relative to the experimental one.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer