Title: Converting Core Strengths to Equivalent Specified Concrete Strengths

Author(s): F. Michael Bartlett

Publication: Concrete International

Volume: 46

Issue: 11

Appears on pages(s): 43-47

Keywords: method, factor, variation, deviation

DOI:

Date: 11/1/2024

Abstract:
ACI PRC-214.4-21 and ACI CODE-562-21 provide methods for converting concrete core strength test results into equivalent specified concrete strengths. The research discussed in this paper investigates the applicability of these methods as well as their limitations.




  