Title: The Measurement Context of Carbon Content Quantification

Author(s): Edward Garboczi, Bruce Scruggs, Alexander K. Landauer, and Prannoy Suraneni

Publication: Concrete International

Volume: 46

Issue: 12

Appears on pages(s): 45-49

Keywords: material, method, technique, specification

DOI:

Date: 12/1/2024

Abstract:
Efforts to optimize current materials and processes, and to develop new cementitious materials and technologies that can meet specific reduction criteria are underway in industry, government, and academia. Validating claims of reduced embodied carbon relies on demonstrating, quantitatively and accurately with known uncertainty, that a material or process meets these criteria.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer