Title: Investigation of Applicability of Non-sintered Cement Mortar for Precast Concrete by Steam Curing

Author(s): Hyeong-Won Na & Won-Gil Hyung

Publication: IJCSM

Volume: 18

Issue:

Appears on pages(s):

Keywords: Blast furnace slag, Fly ash, Non-sintered cement, Precast concrete

DOI: 10.1186/s40069-024-00689-6

Date: 9/30/2024

Abstract:
Non-sintered cement (NSC) mortar was developed using only industrial by-products, such as ground granulated blast furnace slag, classes C and F fly ashes, and slaked lime. The characteristics of different NSC mortar formulations were investigated, as well as their applicability for use in forming precast concrete products. X-ray diffraction and scanning electron microscope analyses were performed to examine the internal structure of the different formulations. Overall, the developed NSC mortar satisfied the existing quality standards in terms of strength performance and absorption rate. Therefore, it is expected to be highly applicable as a raw material for production of the desired cement products.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer